Euronorm EN EN X3CrNiM0NB17-13-3 Euronorm Stainless Steel and EN X3CrNiM0NB17-13-3 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X3CrNiM0NB17-13-3 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiMaCuWN25-7-4 |
|||||
EN X2CrNiM0Ni7-13-3 |
|||||
EN X2CrNiM0N17-13-5 |
|||||
EN X2CrNiM0N22-5-3 |
|||||
EN X2CrNiM0N25-7-4 |
|||||
EN X2CrNiM0Si18-5-3 |
|||||
EN X2CrNiNi8-10 |
|||||
EN X2CrNiN23-4 |
|||||
EN X2NiCrAlTi32-20 |
|||||
EN X3CrNiM017-13-3 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | B(%) |
---|---|---|---|---|---|---|---|---|---|
0.04 | 0.75 | 2.00 | 0.035 | 0.015 | 16.0-18.0 | 12.0-14.0 | 2.00-3.00 | 0.10-0.18 | 0.0015-0.005 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
716 (≥) | 491 (≥) | 14 | 43 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.23 | - | |||
924 | 749 | - | 33.3 | 321 | - | ||
823 | - | 14 | 24.2 | 213 | 214 |
Heat treated : 1296°C - 1423°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X3CrNiM0NB17-13-3 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com