Euronorm EN EN X2NiCrAlTi32-20 Euronorm Stainless Steel and EN X2NiCrAlTi32-20 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X2NiCrAlTi32-20 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiM018-14-3 |
|||||
EN X2CrNiM0CuN26-6-3 |
|||||
EN X2CrNiMaCuWN25-7-4 |
|||||
EN X2CrNiM0Ni7-13-3 |
|||||
EN X2CrNiM0N17-13-5 |
|||||
EN X2CrNiM0N22-5-3 |
|||||
EN X2CrNiM0N25-7-4 |
|||||
EN X2CrNiM0Si18-5-3 |
|||||
EN X2CrNiNi8-10 |
|||||
EN X2CrNiN23-4 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) | Al(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|
0.030 | 0.70 | 1.00 | 0.020 | 0.015 | 20.0-23.0 | 32.0-35.0 | 0.10-0.60 | 0.15-0.45 | 8X(C+N)-0.60 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
874 (≥) | 365 (≥) | 41 | 11 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.12 | - | |||
923 | 858 | - | 41.3 | 143 | - | ||
185 | - | 21 | 13.2 | 332 | 442 |
Heat treated : 1791°C - 1743°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X2NiCrAlTi32-20 | EN | Euronorm | Euronorm Stainless Steel |