Euronorm EN EN X2CrNiNi8-10 Euronorm Stainless Steel and EN X2CrNiNi8-10 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNi18-9 |
|||||
EN X2CrNiCu19-10 |
|||||
EN X2CrNiMo17-12-2 |
|||||
EN X2CrNiMo17-12-3 |
|||||
EN X2CrNiMo18-14-3 |
|||||
EN X2CrNiMoN225-3 |
|||||
EN X2CrNiMoN1M1-2 |
|||||
EN X2CrNiMoN17-13-3 |
|||||
EN X2CrNiMoN17-13-5 |
|||||
EN X2CrNiMoN25-7-4 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
854 (≥) | 158 (≥) | 31 | 44 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
33 | - | - | 0.32 | - | |||
795 | 648 | - | 11.3 | 143 | - | ||
379 | - | 13 | 14.2 | 123 | 223 |
Heat treated : 1326°C - 1575°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiNi8-10 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com