Euronorm EN EN X2CrNiM0Ni7-13-3 Euronorm Stainless Steel and EN X2CrNiM0Ni7-13-3 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X2CrNiM0Ni7-13-3 | EN | Euronorm | Euronorm Stainless Steel |
EN X1CrNiMoN25-22-2 |
|||||
EN X1NiCrMoCu25-20-5 |
|||||
EN X1NiCrMoCu31-27-4 |
|||||
EN X1NiCrMoCuN25-20-7 |
|||||
EN X2CrNi18-9 |
|||||
EN X2CrNi19-11 |
|||||
EN X2CrNiM017-12-2 |
|||||
EN X2CrNiM018-14-3 |
|||||
EN X2CrNiM0CuN26-6-3 |
|||||
EN X2CrNiMaCuWN25-7-4 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
0.030 | 1.00 | 2.00 | 0.040 | 0.015 | 16.5-18.5 | 11.0-14.0 | 12.50-3.00 | 0.12-0.22 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
969 (≥) | 278 (≥) | 21 | 31 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.34 | - | |||
182 | 585 | - | 12.3 | 111 | - | ||
537 | - | 32 | 43.2 | 134 | 213 |
Heat treated : 1954°C - 1111°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X2CrNiM0Ni7-13-3 | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com