Japan DAIDO LAK52 不锈钢 and Mechanical Properties, Chemical Element, Cross Reference.
Element | Min | Max | Similar |
---|---|---|---|
特殊元素 | - | - | - |
Mo | - | - | 1.0000 |
Cr | - | - | 20.0000 |
Mn | - | - | 0.3000 |
Si | - | - | 0.1500 |
C | - | - | 0.0100 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
598 (≥) | 882 (≥) | 31 | 13 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.11 | - | |||
743 | 514 | - | 21.3 | 314 | - | ||
421 | - | 14 | 42.2 | 232 | 212 |
Heat treated : 1985°C - 1234°C
Grade | Standard | Country | Application |
---|---|---|---|
ASTM 5140 | |||
AISI 201 | |||
AISI 202 | |||
1.2767 | |||
17-4PH | |||
AISI 1052 | |||
AISI 416Se | |||
AISI 1330 | |||
AISI 205 Stainless Steel | |||
AISI A10 | |||
AISI A2 | |||
AISI A3 | |||
AISI A4 | |||
1.0036 | |||
1.0037 | |||
SAE J403 | |||
UNS G10100 | |||
AMS 4924 | |||
ASTM A36 | |||
Electrode 100S-1 |