Available 24/7 at contact@steel-grades.com

Japan DAIDO DAPKCW3 表面硬化用粉末 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: DAPKCW3 / DAP KCW3
Category Grade Standard Region/Area Standard Content
Metals DAP KCW3 DAIDO PFSH Japan 表面硬化用粉末

Chemical composition(mass fraction)(wt.%) of the DAP KCW3

Element Min Max Similar
Fe - - 1.5000
W - - 8.0000
Mo - - 0.6000
Cr - - 30.0000
Ni - - 1.5000
Si - - 1.1000
C - - 1.5000

Mechanical Properties of steel grade DAP KCW3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
936 (≥) 268 (≥) 14 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical Properties of steel grade DAP KCW3

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.41 -  
447 771 - 12.3 443   -  
961 - 21 23.2   213 234

Heat Treatment of steel grade DAP KCW3

Heat treated : 1415°C - 1736°C

Technological Curves of steel grade DAP KCW3

Cross Reference Table (Equivalent Grade) of DAP KCW3

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this DAP KCW3?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top