Germany DIN NiCr19Fe19Nb5Mo3 抗蠕变钢,镍和钴合金 and Mechanical Properties, Chemical Element, Cross Reference.
Category | Grade | Standard | Region/Area | Standard Content |
---|---|---|---|---|
Metals | NiCr19Fe19Nb5Mo3 | DIN EN 10302 | Germany | 抗蠕变钢,镍和钴合金 |
Element | Min | Max | Similar |
---|---|---|---|
Fe | - | - | - |
Ti | 0.6000 | 1.2000 | - |
Nb | 4.7000 | 5.5000 | - |
Co | - | 1.0000 | - |
Cu | - | 0.3000 | - |
Ni | 50.0000 | 55.0000 | - |
Mo | 2.8000 | 3.3000 | - |
Cr | 17.0000 | 21.0000 | - |
B | 0.0020 | 0.0060 | - |
Al | 0.3000 | 0.7000 | - |
S | - | 0.0150 | - |
P | - | 0.0150 | - |
Mn | - | 0.0350 | - |
Si | - | 0.0350 | - |
C | 0.0200 | 0.0800 | - |
C | 0.0200 | 0.0800 | - |
Mn | - | 0.3500 | - |
P | - | 0.0150 | - |
S | - | 0.0150 | - |
Si | - | 0.3500 | - |
Ni | 50.0000 | 55.0000 | - |
Cr | 17.0000 | 21.0000 | - |
Mo | 2.8000 | 3.3000 | - |
Cu | - | 0.3000 | - |
Ti | 0.6000 | 1.2000 | - |
B | 0.0020 | 0.0060 | - |
Al | 0.3000 | 0.7000 | - |
Fe | - | - | - |
Co | - | 1.0000 | - |
Nb+Ta | 4.7000 | 5.5000 | - |
Ti | 0.6000 | 1.2000 | - |
Si | - | 0.3500 | - |
S | - | 0.0150 | - |
P | - | 0.0150 | - |
Ni | 50.0000 | 55.0000 | - |
Nb+Ta | 4.7000 | 5.5000 | - |
Mo | 2.8000 | 3.3000 | - |
Mn | - | 0.3500 | - |
Fe | - | - | - |
Cu | - | 0.3000 | - |
Cr | 17.0000 | 21.0000 | - |
Co | - | 1.0000 | - |
C | 0.0200 | 0.0800 | - |
B | - | 0.0060 | - |
Al | 0.3000 | 0.7000 | - |
Ti | 0.6000 | 1.2000 | - |
Si | - | 0.3500 | - |
S | - | 0.0150 | - |
P | - | 0.0150 | - |
Ni | 50.0000 | 55.0000 | - |
Nb+Ta | 4.7000 | 5.5000 | - |
Mo | 2.8000 | 3.3000 | - |
Mn | - | 0.3500 | - |
Fe | - | - | - |
Cu | - | 0.3000 | - |
Cr | 17.0000 | 21.0000 | - |
Co | - | 1.0000 | - |
C | 0.0200 | 0.0800 | - |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
856 (≥) | 911 (≥) | 31 | 33 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.12 | - | |||
174 | 717 | - | 43.3 | 212 | - | ||
969 | - | 32 | 23.2 | 211 | 221 |
Heat treated : 1464°C - 1914°C
Grade | Standard | Country | Application |
---|---|---|---|
ASTM 5140 | |||
AISI 201 | |||
AISI 202 | |||
1.2767 | |||
17-4PH | |||
AISI 1052 | |||
AISI 416Se | |||
AISI 1330 | |||
AISI 205 Stainless Steel | |||
AISI A10 | |||
AISI A2 | |||
AISI A3 | |||
AISI A4 | |||
1.0036 | |||
1.0037 | |||
SAE J403 | |||
UNS G10100 | |||
AMS 4924 | |||
ASTM A36 | |||
Electrode 100S-1 |