Chemical composition(mass fraction)(wt.%) of the S 275 JRC

Element Min Max Similar
S - 0.0550 -
P - 0.0550 -
N - 0.0110 -
Mn - 1.6000 -
C - 0.2400 -
Al - - -

Mechanical Properties of steel grade S 275 JRC

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
519 (≥) 377 (≥) 42 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical Properties of steel grade S 275 JRC

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
11 - -     0.43 -  
382 936 - 23.3 343   -  
371 - 23 42.2   222 131

Heat Treatment of steel grade S 275 JRC

Heat treated : 1593°C - 1926°C

Technological Curves of steel grade S 275 JRC

Cross Reference Table (Equivalent Grade) of S 275 JRC

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this S 275 JRC?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top