Category Grade Standard Region/Area Standard Content
Metals 1.7227 EN 10083-1 EU 淬火和回火钢 - 第1部分:一般交货技术条件

Chemical composition(mass fraction)(wt.%) of the 1.7227

Element Min Max Similar
Si - 0.3000 -
S 0.0200 0.0400 -
P - 0.0250 -
Mo 0.1500 0.3000 -
Mn 0.6000 0.9000 -
Cu - 0.2500 -
Cr 0.9000 1.2000 -
C 0.3800 0.4500 -
Si - 0.4000 -
S 0.0200 0.0400 -
P - 0.0350 -
Mo 0.1500 0.3000 -
Mn 0.6000 0.9000 -
Cr 0.9000 1.2000 -
C 0.3800 0.4500 -

Mechanical Properties of steel grade 1.7227

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
124 (≥) 692 (≥) 14 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical Properties of steel grade 1.7227

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
14 - -     0.11 -  
679 714 - 43.3 222   -  
865 - 11 11.2   334 423

Heat Treatment of steel grade 1.7227

Heat treated : 1135°C - 1696°C

Technological Curves of steel grade 1.7227

Cross Reference Table (Equivalent Grade) of 1.7227

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 1.7227?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top