Austria ONORM UC12 Wire rod from unalloyed steel for cold drawing; quality specification and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: UC12 / UC 12
Category Grade Standard Region/Area Standard Content
Metals UC 12 ÖNORM M3110 Austria Wire rod from unalloyed steel for cold drawing; quality specification

Chemical composition(mass fraction)(wt.%) of the UC 12

Element Min Max Similar
S - 0.0400 -
P+S - 0.0700 -
P - 0.0400 -
Mn - 0.5000 -
C 0.0800 0.1200 -

Mechanical Properties of steel grade UC 12

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
146 (≥) 995 (≥) 43 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical Properties of steel grade UC 12

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.22 -  
268 535 - 42.3 212   -  
357 - 13 32.2   133 211

Heat Treatment of steel grade UC 12

Heat treated : 1337°C - 1443°C

Technological Curves of steel grade UC 12

Cross Reference Table (Equivalent Grade) of UC 12

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this UC 12?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top