UK X3CrNiM0N27-5-2 austenitic special steel and X3CrNiM0N27-5-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X3CrNiM0N27-5-2 | UK | austenitic special steel | |
1.4578 |
|||||
1.4563 |
|||||
X1NiCrM0Cu31-27-4 |
|||||
1.4537 |
|||||
X1CrNiM0CuN25-25-5 |
|||||
X1CrNiM0CUN20-18-7 |
|||||
1.4547 |
|||||
1.4529 |
|||||
X1NiCrM0CuN25-20-7 |
|||||
1.4460 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
Max 0.050 | Max 1.00 | Max 2.00 | Max 0.035 | Max 0.015① | 25.0-28.0 | 4.50-6.50 | 1.30-2.00 | 0.05-0.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
813 (≥) | 333 (≥) | 42 | 22 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
14 | - | - | 0.11 | - | |||
721 | 618 | - | 34.3 | 231 | - | ||
249 | - | 43 | 12.2 | 334 | 232 |
Heat treated : 1725°C - 1978°C
Grade | Standard | Country | Application |
---|---|---|---|
X3CrNiM0N27-5-2 | UK | austenitic special steel |