UK 1.4578 austenitic special steel and 1.4578 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | 1.4578 | UK | austenitic special steel | |
1.4580 |
|||||
X2CrNiM0l8-15-4 |
|||||
1.4438 |
|||||
X1CrNiSil8-15-4 |
|||||
1.4361 |
|||||
1.4560 |
|||||
X3CrNiCul9-9-2 |
|||||
X6CrNiCuSl8-9-2 |
|||||
1.4570 |
|||||
X3CrNiCuM0l7-11-3-2 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
Max 0.040 | Max 1.00 | Max 1.00 | Max 0.045 | Max 0.015 | 16.5-17.5 | 10.0-11.0 | 2.00-2.50 | Max 0.11 | 3.00-3.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
937 (≥) | 274 (≥) | 22 | 24 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.14 | - | |||
152 | 826 | - | 43.3 | 411 | - | ||
399 | - | 32 | 11.2 | 341 | 222 |
Heat treated : 1632°C - 1355°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...