C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
Max 0.020 | Max 0.70 | Max 1.00 | Max 0.03 | Max 0.010 | 19.5-20.5 | 17.5-18.5 | 6.00-7.00 | 0.18-0.25 | 0.50-1.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
838 (≥) | 787 (≥) | 13 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
42 | - | - | 0.44 | - | |||
558 | 594 | - | 12.3 | 313 | - | ||
138 | - | 42 | 34.2 | 442 | 421 |
Heat treated : 1291°C - 1319°C
Grade | Standard | Country | Application |
---|---|---|---|
1.4547 | UK | austenitic special steel | |
1.4547(AFNOR) | AFNOR | France | Austenite |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com