Germany DIN 1.4743 Heat resistant steel castings and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: 1.4743 / 1.4743
Category Grade Standard Region/Area Standard Content
Metals 1.4743 DIN EN 10295 Germany Heat resistant steel castings

Chemical composition(mass fraction)(wt.%) of the 1.4743

Element Min Max Similar
Si 1.0000 2.5000 -
S - 0.0300 -
P - 0.0450 -
Mn 0.5000 1.0000 -
Cr 17.0000 19.0000 -
C 1.4000 1.8000 -

Mechanical Properties of steel grade 1.4743

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
766 (≥) 992 (≥) 33 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical Properties of steel grade 1.4743

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
13 - -     0.42 -  
745 968 - 24.3 222   -  
477 - 12 34.2   442 343

Heat Treatment of steel grade 1.4743

Heat treated : 1165°C - 1348°C

Technological Curves of steel grade 1.4743

Cross Reference Table (Equivalent Grade) of 1.4743

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 1.4743?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top