Metals DAP RC276 DAIDO HRACRSP Japan 耐热耐蚀性超合金粉末

Chemical composition(mass fraction)(wt.%) of the DAP RC276

Element Min Max Similar
W - - 4.0000
Fe - - 5.0000
Mo - - 16.0000
Cr - - 15.5000
C - 0.0100 -

Mechanical Properties of steel grade DAP RC276

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
778 (≥) 236 (≥) 42 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical Properties of steel grade DAP RC276

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
33 - -     0.21 -  
327 267 - 13.3 222   -  
349 - 11 43.2   311 221

Heat Treatment of steel grade DAP RC276

Heat treated : 1684°C - 1387°C

Technological Curves of steel grade DAP RC276

Cross Reference Table (Equivalent Grade) of DAP RC276

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this DAP RC276?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top