Category Grade Standard Region/Area Standard Content
Metals DAP KCN1 DAIDO PFSH Japan 表面硬化用粉末

Chemical composition(mass fraction)(wt.%) of the DAP KCN1

Element Min Max Similar
Fe - - 1.5000
W - - 12.0000
Mo - - 0.6000
Cr - - 26.0000
Ni - - 22.0000
Si - - 1.1000
C - - 1.8000

Mechanical Properties of steel grade DAP KCN1

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
162 (≥) 228 (≥) 43 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical Properties of steel grade DAP KCN1

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.42 -  
747 629 - 34.3 114   -  
766 - 31 24.2   432 423

Heat Treatment of steel grade DAP KCN1

Heat treated : 1447°C - 1894°C

Technological Curves of steel grade DAP KCN1

Cross Reference Table (Equivalent Grade) of DAP KCN1

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this DAP KCN1?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top