Datasheet for: Metals: C35E / C 35 E
Category Grade Standard Region/Area Standard Content
Metals C 35 E DIN EN 10132-3 Germany 热处理冷轧窄钢带- 交货技术条件 - 第3部分:淬火和回火钢

Chemical composition(mass fraction)(wt.%) of the C 35 E

Element Min Max Similar
Cr+Mo+Ni - 0.6300 -
Ni - 0.4000 -
Mo - 0.1000 -
Cr - 0.4000 -
S - 0.0150 -
P - 0.0300 -
Mn 0.5000 0.8000 -
Si - 0.4000 -
C 0.3200 0.3900 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0300 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr+Mo+Ni - 0.6300 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0300 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.4000 0.7000 -
Cr+Mo+Ni - 0.6300 -
Cr - 0.4000 -
C 0.1700 0.2400 -
Cr+Mo+Ni - 0.6300 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0300 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0350 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr+Mo+Ni - 0.6300 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Cr+Mo+Ni - 0.6300 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0350 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0350 -
Other - - -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr+Mo+Ni - 0.6300 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Cr+Mo+Ni - 0.6300 -
Si - 0.4000 -
S - 0.0150 -
P - 0.0300 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr - 0.4000 -
C 0.3200 0.3900 -
Si - 0.4000 -
S - 0.0350 -
P - 0.0350 -
Ni - 0.4000 -
Mo - 0.1000 -
Mn 0.5000 0.8000 -
Cr - 0.4000 -
C 0.3200 0.3900 -

Mechanical Properties of steel grade C 35 E

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
433 (≥) 278 (≥) 41 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical Properties of steel grade C 35 E

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.34 -  
573 125 - 33.3 114   -  
576 - 43 22.2   433 242

Heat Treatment of steel grade C 35 E

Heat treated : 1861°C - 1423°C

Technological Curves of steel grade C 35 E

Cross Reference Table (Equivalent Grade) of C 35 E

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this C 35 E?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top