Sweden SS 1774 弹簧钢 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: 1774 / 1774
Category Grade Standard Region/Area Standard Content
Metals 1774 SS 141774 Sweden 弹簧钢

Chemical composition(mass fraction)(wt.%) of the 1774

Element Min Max Similar
Si 0.1500 0.4000 -
S - 0.0350 -
P - 0.0350 -
Mn 0.3000 0.8000 -
C 0.6000 0.9500 -

Mechanical Properties of steel grade 1774

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
797 (≥) 744 (≥) 21 43 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical Properties of steel grade 1774

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.41 -  
154 995 - 24.3 132   -  
418 - 32 21.2   321 223

Heat Treatment of steel grade 1774

Heat treated : 1414°C - 1791°C

Technological Curves of steel grade 1774

Cross Reference Table (Equivalent Grade) of 1774

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 1774?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top