Sweden SS 2343-12 Stainless steel - SS steel 23 43 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: 2343-12 / 2343-12
Category Grade Standard Region/Area Standard Content
Metals 2343-12 SS 142343 Sweden Stainless steel - SS steel 23 43

Chemical composition(mass fraction)(wt.%) of the 2343-12

Element Min Max Similar
Si - 1.0000 -
S - 0.0300 -
P - 0.0450 -
Ni 10.5000 14.0000 -
Mo 2.5000 3.0000 -
Mn - 2.0000 -
Cr 16.0000 18.5000 -
C - 0.0500 -

Mechanical Properties of steel grade 2343-12

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
643 (≥) 979 (≥) 11 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical Properties of steel grade 2343-12

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
33 - -     0.32 -  
739 931 - 13.3 313   -  
794 - 41 14.2   431 243

Heat Treatment of steel grade 2343-12

Heat treated : 1887°C - 1341°C

Technological Curves of steel grade 2343-12

Cross Reference Table (Equivalent Grade) of 2343-12

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 2343-12?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top