Available 24/7 at contact@steel-grades.com

America UNS W43070 合成热喷涂钢丝 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: W43070 / W43070
Category Grade Standard Region/Area Standard Content
Metals W43070 -- America 合成热喷涂钢丝

Chemical composition(mass fraction)(wt.%) of the W43070

Element Min Max Similar
Si - 1.0000 -
Mo - 0.7500 -
Mn - 1.0000 -
Cr 16.0000 18.0000 -
C 0.6000 0.8000 -

Mechanical Properties of steel grade W43070

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
466 (≥) 343 (≥) 34 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical Properties of steel grade W43070

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
32 - -     0.33 -  
628 716 - 44.3 312   -  
521 - 42 32.2   124 141

Heat Treatment of steel grade W43070

Heat treated : 1848°C - 1684°C

Technological Curves of steel grade W43070

Cross Reference Table (Equivalent Grade) of W43070

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this W43070?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top