Chemical composition(mass fraction)(wt.%) of the C 4751

Element Min Max Similar
W - - 0.3500
V - - 0.4100
Si - - 1.0000
S - - 0.0070
P - - 0.0300
Ni - - 0.2400
Mo - - 1.2800
Mn - - 0.3500
Cu - - 0.2500
Cr - - 5.0600
C - - 0.4200

Mechanical Properties of steel grade C 4751

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
235 (≥) 952 (≥) 42 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical Properties of steel grade C 4751

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
22 - -     0.23 -  
231 759 - 33.3 443   -  
967 - 11 32.2   233 444

Heat Treatment of steel grade C 4751

Heat treated : 1119°C - 1378°C

Technological Curves of steel grade C 4751

Cross Reference Table (Equivalent Grade) of C 4751

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this C 4751?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top