Available 24/7 at contact@steel-grades.com

BÖHLER T262 EXTRA

Global 企业标准 BÖHLERT262EXTRA and Mechanical Properties, Chemical Element, Cross Reference.

Category Grade Standard Region/Area Standard Content
Metals BÖHLER T262 EXTRA -- Global

Chemical composition(mass fraction)(wt.%) of the BÖHLER T262 EXTRA

Element Min Max Similar

Mechanical Properties of steel grade BÖHLER T262 EXTRA

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
555 (≥) 188 (≥) 32 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical Properties of steel grade BÖHLER T262 EXTRA

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
41 - -     0.43 -  
618 954 - 14.3 231   -  
988 - 14 34.2   431 412

Heat Treatment of steel grade BÖHLER T262 EXTRA

Heat treated : 1953°C - 1893°C

Technological Curves of steel grade BÖHLER T262 EXTRA

Cross Reference Table (Equivalent Grade) of BÖHLER T262 EXTRA

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this BÖHLER T262 EXTRA?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account