Available 24/7 at contact@steel-grades.com

Global 企业标准 KATO3 and Mechanical Properties, Chemical Element, Cross Reference.

Datasheet for: Metals: KATO3 / KATO3
Category Grade Standard Region/Area Standard Content
Metals KATO3 -- Global

Chemical composition(mass fraction)(wt.%) of the KATO3

Element Min Max Similar
Si - 0.2500 -
Ni - 2.7500 -
Mn - 0.4800 -
Cr - 0.7500 -
C - 0.3100 -

Mechanical Properties of steel grade KATO3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
822 (≥) 564 (≥) 13 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical Properties of steel grade KATO3

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
13 - -     0.11 -  
772 453 - 14.3 332   -  
688 - 34 42.2   441 331

Heat Treatment of steel grade KATO3

Heat treated : 1912°C - 1696°C

Technological Curves of steel grade KATO3

Cross Reference Table (Equivalent Grade) of KATO3

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this KATO3?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top