Chemical composition(mass fraction)(wt.%) of the 1.6746

Element Min Max Similar
Si 0.1500 0.3500 -
S - 0.0350 -
P - 0.0350 -
Ni 3.0000 3.8000 -
Mo 0.3500 0.5500 -
Mn 0.3000 0.6000 -
Cr 1.0000 1.5000 -
C 0.2800 0.3600 -

Mechanical Properties of steel grade 1.6746

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
248 (≥) 193 (≥) 32 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical Properties of steel grade 1.6746

Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson’s coefficient, ν
24 - -     0.22 -  
735 249 - 23.3 343   -  
656 - 32 42.2   311 232

Heat Treatment of steel grade 1.6746

Heat treated : 1569°C - 1654°C

Technological Curves of steel grade 1.6746

Cross Reference Table (Equivalent Grade) of 1.6746

Available Suppliers

Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...

Rfq.: sales@longhaisteel.com
  • Do you supply this 1.6746?
  • List your company on S&G now? Join
  • Non-paying users only
Sidebar RFQs Menu My Account
Top