Romania STAS/SR 20MnCr12XS Alloy structural steel and 20MnCr12XS Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | 20MnCr12XS | STAS/SR | Romania | Alloy structural steel |
| 18MnCr11S |
|||||
| 18MnCr11X |
|||||
| 18MnCr11XS |
|||||
| 19MoCr11 |
|||||
| !9MoCr11S |
|||||
| 19MoCr11X |
|||||
| 19MoCr11XS |
|||||
| 20MnCr12 |
|||||
| 20MnCr12S |
|||||
| 20MnCr12X |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Ti(%) |
|---|---|---|---|---|---|---|---|---|---|
| 0.17-0,22 | 0.17-0.37 | 2.10-1.40 | 0.025 | 0.020-0.035 | 1.00- 1.30 | 0.3 | 0.15 | 0.3 | 0.02 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 754 (≥) | 587 (≥) | 44 | 41 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 41 | - | - | 0.44 | - | |||
| 624 | 144 | - | 13.3 | 212 | - | ||
| 746 | - | 22 | 34.2 | 214 | 121 |
Heat treated : 1212°C - 1595°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 20MnCr12XS | STAS/SR | Romania | Alloy structural steel |