| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Ti(%) |
|---|---|---|---|---|---|---|---|---|---|
| 0.15-0.21 | 0.17-0.37 | 0.90-1.20 | 0.025 | 0.020-0.035 | 0.90-1.20 | 0.3 | 0.15 | 0.30 | 0.02 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 299 (≥) | 565 (≥) | 23 | 34 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.24 | - | |||
| 898 | 663 | - | 13.3 | 444 | - | ||
| 887 | - | 41 | 32.2 | 312 | 314 |
Heat treated : 1113°C - 1564°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 18MnCr11XS | STAS/SR | Romania | Alloy structural steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com