Romania STAS/SR 19MoCr11 Alloy structural steel and 19MoCr11 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Structure Steel | 19MoCr11 | STAS/SR | Romania | Alloy structural steel |
17MoCrNi14X |
|||||
17MoCrNi14XS |
|||||
18CrNi20 |
|||||
18CrNi20S |
|||||
18CrNi20X |
|||||
18CrNi20XS |
|||||
18MnCr11 |
|||||
18MnCr11S |
|||||
18MnCr11X |
|||||
18MnCr11XS |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|
0.16-0.22 | 0.17-0.37 | 0.60-0.90 | 0.035 | 0.035 | 0.90-1.20 | 0.3 | 0.15-0.25 | 0.3 | 0.02 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
422 (≥) | 554 (≥) | 13 | 32 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.22 | - | |||
248 | 672 | - | 33.3 | 342 | - | ||
339 | - | 34 | 22.2 | 134 | 131 |
Heat treated : 1661°C - 1419°C
Grade | Standard | Country | Application |
---|---|---|---|
19MoCr11 | STAS/SR | Romania | Alloy structural steel |
19MoCr11X | STAS/SR | Romania | Alloy structural steel |
19MoCr11XS | STAS/SR | Romania | Alloy structural steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com