France AFNOR Z3CNDU25-07Az Stainless Steel Plate & Steel Strip and Z3CNDU25-07Az Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | Z3CNDU25-07Az | AFNOR | France | Stainless Steel Plate & Steel Strip |
Z3CND18-12-03 |
|||||
Z3CND18-14-03 |
|||||
Z3CND18-14-05Az |
|||||
Z3CND19-14Az |
|||||
Z3CND19-15-04 |
|||||
Z3CND22-05Az |
|||||
Z3CND25-06Az |
|||||
Z3CND25-07Az |
|||||
Z3CNDU22-07Az |
|||||
Z3CNDU25-06Az |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
Max 0.03 | Max 0.75 | Max 2.00 | Max 0.035 | Max 0.010 | 24.0-26.0 | 5.50-7.50 | 2.70-3.90 | 0.14-0.25 | 1.00-2.50 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
442 (≥) | 173 (≥) | 13 | 14 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 211 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.44 | - | |||
917 | 468 | - | 42.3 | 214 | - | ||
867 | - | 34 | 24.2 | 233 | 214 |
Heat treated : 1672°C - 1814°C
Grade | Standard | Country | Application |
---|---|---|---|
Z3CNDU25-07Az | AFNOR | France | Stainless Steel Plate & Steel Strip |