France AFNOR Z3CND18-14-05Az Stainless Steel Plate & Steel Strip and Z3CND18-14-05Az Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | Z3CND18-14-05Az | AFNOR | France | Stainless Steel Plate & Steel Strip |
Z3CN18-10 |
|||||
Z3CN18-10Az |
|||||
Z3CN23-04Az |
|||||
Z3CND17-11Az |
|||||
Z3CND17-11-01 |
|||||
Z3CND17-11-02 |
|||||
Z3CND17-12Az |
|||||
Z3CND17-12-03 |
|||||
Z3CND18-12-03 |
|||||
Z3CND18-14-03 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
Max 0.03 | Max 0.75 | Max 2.00 | Max 0.035 | Max 0.010 | 17.0-19.0 | 13.0-15.0 | 4.00-5.00 | 0.12-0.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
222 (≥) | 185 (≥) | 33 | 11 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.24 | - | |||
874 | 146 | - | 23.3 | 144 | - | ||
788 | - | 43 | 31.2 | 414 | 423 |
Heat treated : 1243°C - 1149°C
Grade | Standard | Country | Application |
---|---|---|---|
Z3CND18-14-05Az | AFNOR | France | Stainless Steel Plate & Steel Strip |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com