France AFNOR Z11CN18-08 Stainless Steel Plate & Steel Strip and Z11CN18-08 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | Z11CN18-08 | AFNOR | France | Stainless Steel Plate & Steel Strip |
Z6CN19-09Az |
|||||
Z6CND16-05-01 |
|||||
Z6CND18-12-03 |
|||||
Z8CN17 |
|||||
Z8CN25-20 |
|||||
Z8CNT12 |
|||||
Z9CNA17-07 |
|||||
Z10CNDA15-07 |
|||||
Z10NC32-21 |
|||||
Z11CN17-08 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) |
---|---|---|---|---|---|---|
0.09-0.12 | Max 0.75 | 0.75-1.20 | Max 0.040 | Max 0.015 | 16.5-18.5 | 7.00-8.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
425 (≥) | 759 (≥) | 34 | 41 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.23 | - | |||
539 | 874 | - | 21.3 | 333 | - | ||
918 | - | 11 | 12.2 | 134 | 313 |
Heat treated : 1766°C - 1218°C
Grade | Standard | Country | Application |
---|---|---|---|
Z11CN18-08 | AFNOR | France | Stainless Steel Plate & Steel Strip |