C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) |
---|---|---|---|---|---|---|
0.09-0.12 | Max 0.75 | 0.75-1.20 | Max 0.040 | Max 0.015 | 16.5-17.5 | 7.00-8.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
217 (≥) | 558 (≥) | 12 | 34 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.34 | - | |||
764 | 232 | - | 24.3 | 123 | - | ||
176 | - | 44 | 23.2 | 434 | 421 |
Heat treated : 1899°C - 1676°C
Grade | Standard | Country | Application |
---|---|---|---|
Z11CN17-08 | AFNOR | France | Stainless Steel Plate & Steel Strip |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com