C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
---|---|---|---|---|---|---|---|
Max 0.06 | Max 0.75 | Max 2.00 | Max 0.040 | Max 0.015 | 16.5-18.5 | 11.0-13.0 | 2.25-2.75 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
475 (≥) | 584 (≥) | 12 | 34 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
11 | - | - | 0.21 | - | |||
691 | 524 | - | 24.3 | 244 | - | ||
955 | - | 44 | 22.2 | 433 | 424 |
Heat treated : 1199°C - 1311°C
Grade | Standard | Country | Application |
---|---|---|---|
Z6CND18-12-03 | AFNOR | France | Stainless Steel Plate & Steel Strip |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com