Germany DIN X8(12)CrNi25-21 Stainless steel and X8(12)CrNi25-21 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X8(12)CrNi25-21 | DIN | Germany | Stainless steel |
X10CrAISi25/X10CrAI24 |
|||||
1.4821 |
|||||
X15(20)CrNiSi25-4 |
|||||
1.4828 |
|||||
X15CrNiSi20-12 |
|||||
1.4833 |
|||||
X12CrNi23-13/X7CrNi23-14 |
|||||
1.4841 |
|||||
X15CrNiSi25-21(20) |
|||||
1.4845 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) |
---|---|---|---|---|---|---|---|
Max 0.10 | Max 1.50 | Max 2.00 | Max 0.045 | Max 0.015 | 24.0-26.0 | 24.0-26.0 | Max 0.11 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
421 (≥) | 698 (≥) | 21 | 23 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.34 | - | |||
834 | 135 | - | 44.3 | 133 | - | ||
458 | - | 14 | 41.2 | 214 | 144 |
Heat treated : 1768°C - 1373°C
Grade | Standard | Country | Application |
---|---|---|---|
X8(12)CrNi25-21 | DIN | Germany | Stainless steel |