Germany DIN X15(20)CrNiSi25-4 Stainless steel and X15(20)CrNiSi25-4 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X15(20)CrNiSi25-4 | DIN | Germany | Stainless steel |
1.4720 |
|||||
1.4724 |
|||||
X10CrAISi13/X10CrAI13 |
|||||
1.4742 |
|||||
X10CrAISi18/X10CrAI18 |
|||||
X18CrN28 |
|||||
1.4749 |
|||||
1.4762 |
|||||
X10CrAISi25/X10CrAI24 |
|||||
1.4821 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) |
---|---|---|---|---|---|---|---|
0.10-0.20 | 0.80-1.50 | Max 2.00 | Max 0.040 | Max 0.015 | 24.5-27.5 | 3.50-5.50 | Max 0.11 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
496 (≥) | 129 (≥) | 23 | 32 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
44 | - | - | 0.31 | - | |||
293 | 552 | - | 23.3 | 133 | - | ||
981 | - | 21 | 34.2 | 244 | 423 |
Heat treated : 1779°C - 1144°C
Grade | Standard | Country | Application |
---|---|---|---|
X15(20)CrNiSi25-4 | DIN | Germany | Stainless steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...