UK X2CrNiM0Nl7-13-5 austenitic special steel and X2CrNiM0Nl7-13-5 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X2CrNiM0Nl7-13-5 | UK | austenitic special steel | |
X6CrNiM0Til7-12-2 |
|||||
X2CrNiM0l7-12-3 |
|||||
1.4432 |
|||||
1.4429 |
|||||
X2CrNiM0Nl7-13-3 |
|||||
1.4436 |
|||||
X3CrNiM017-13-3 |
|||||
1.4435 |
|||||
X2CrNiM0l8-14-3 |
|||||
1.4439 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
Max 0.030 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.015 | 16.5-18.5 | 12.5-14.5 | 4.00-5.00 | 0.12-0.22 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
239 (≥) | 419 (≥) | 44 | 14 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.41 | - | |||
142 | 288 | - | 14.3 | 321 | - | ||
738 | - | 41 | 34.2 | 343 | 444 |
Heat treated : 1517°C - 1444°C
Grade | Standard | Country | Application |
---|---|---|---|
X2CrNiM0Nl7-13-5 | UK | austenitic special steel |