UK 1.4432 austenitic special steel and 1.4432 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | 1.4432 | UK | austenitic special steel | |
NCF825TP |
|||||
X2CrNiM0l7-12-2 |
|||||
1.4404 |
|||||
X2CrNiM0Nl7-11-2 |
|||||
1.4406 |
|||||
1.4401 |
|||||
X5CrNiM0l7-12-2 |
|||||
1.4571 |
|||||
X6CrNiM0Til7-12-2 |
|||||
X2CrNiM0l7-12-3 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
Max 0.030 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.015 | 16.5-18.0 | 10.5-13.5 | 2.50-3.00 | Max 0.11 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
643 (≥) | 776 (≥) | 41 | 14 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.14 | - | |||
868 | 711 | - | 21.3 | 324 | - | ||
731 | - | 44 | 23.2 | 133 | 421 |
Heat treated : 1651°C - 1969°C
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...