C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|
Max 0.080 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.015 | 16.5-18.5 | 10.5-13.5 | 2.00-2.50 | 5×C-0.70 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
945 (≥) | 428 (≥) | 43 | 41 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
43 | - | - | 0.23 | - | |||
445 | 775 | - | 13.3 | 313 | - | ||
926 | - | 41 | 24.2 | 342 | 111 |
Heat treated : 1674°C - 1516°C
Grade | Standard | Country | Application |
---|---|---|---|
W-Nr 1.4571 | DIN | Germany | Stainless steel |
1.4571 | UK | austenitic special steel | |
1.4571(AFNOR) | AFNOR | France | Austenite |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com