France AFNOR X1CrNiMoCu25-20-5 Austenite and X1CrNiMoCu25-20-5 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X1CrNiMoCu25-20-5 | AFNOR | France | Austenite |
1.4406(AFNOR) |
|||||
X5CrNiMoN17-12-2 |
|||||
1.4401(AFNOR) |
|||||
X6CrNiMoTi17-12-2 |
|||||
1.4571(AFNOR) |
|||||
X2CrNiMo17-12-3 |
|||||
1.4423 |
|||||
X2CrNiMo18-14-3 |
|||||
X2CrNiMoN17-13-5 |
|||||
1.4439(AFNOR) |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | Cu(%) |
---|---|---|---|---|---|---|---|---|---|
Max 0.020 | Max 0.70 | Max 2.00 | Max 0.030 | Max 0.010 | 19.00-21.00 | 24.00-26.00 | 4.00-5.00 | Max 0.15 | 1.20-2.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
989 (≥) | 646 (≥) | 12 | 31 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.24 | - | |||
398 | 862 | - | 13.3 | 124 | - | ||
115 | - | 31 | 12.2 | 112 | 234 |
Heat treated : 1652°C - 1318°C
Grade | Standard | Country | Application |
---|---|---|---|
X1CrNiMoCu25-20-5 | AFNOR | France | Austenite |
ISO X1CrNiMoCu25-20-5 | ISO | ISO | ISO standard thermal deformation of stainless steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...