France AFNOR 1.4423 Austenite and 1.4423 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | 1.4423 | AFNOR | France | Austenite |
1.4303 |
|||||
X2CrNiMo17-12-2 |
|||||
1.4404(AFNOR) |
|||||
X2CrNiMoN17-11-2 |
|||||
1.4406(AFNOR) |
|||||
X5CrNiMoN17-12-2 |
|||||
1.4401(AFNOR) |
|||||
X6CrNiMoTi17-12-2 |
|||||
1.4571(AFNOR) |
|||||
X2CrNiMo17-12-3 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) |
---|---|---|---|---|---|---|---|---|
Max 0.030 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.015 | 16.50-18.50 | 10.50-13.00 | 2.50-3.00 | Max 0.11 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
994 (≥) | 439 (≥) | 32 | 22 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.24 | - | |||
699 | 422 | - | 34.3 | 342 | - | ||
626 | - | 44 | 32.2 | 143 | 323 |
Heat treated : 1223°C - 1259°C