Euronorm EN EN X6CrNiM0Ti17-12-2 Euronorm Stainless Steel and EN X6CrNiM0Ti17-12-2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X6CrNiM0Ti17-12-2 | EN | Euronorm | Euronorm Stainless Steel |
EN X2CrNiN23-4 |
|||||
EN X2NiCrAlTi32-20 |
|||||
EN X3CrNiM017-13-3 |
|||||
EN X3CrNiM0NB17-13-3 |
|||||
EN X5CrNi18-10 |
|||||
EN X5CrNiM017-12-3 |
|||||
EN X5NiCrAlTi31-20 |
|||||
EN X6CrNi18-10 |
|||||
EN X6CrNiM017-13-2 |
|||||
EN X6CrNiM0Nb17-12-2 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|
0.08 | 1.00 | 2.00 | 0.040 | 0-015 | 16.5-18.5 | 10.5-13.5 | 2.00-2.50 | Min5XC-0.7 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
877 (≥) | 535 (≥) | 43 | 43 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
32 | - | - | 0.41 | - | |||
195 | 374 | - | 41.3 | 212 | - | ||
331 | - | 32 | 13.2 | 423 | 141 |
Heat treated : 1244°C - 1253°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X6CrNiM0Ti17-12-2 | EN | Euronorm | Euronorm Stainless Steel |