Euronorm EN EN X2CrNiNi810KD Euronorm Stainless Steel and EN X2CrNiNi810KD Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | EN X2CrNiNi810KD | EN | Euronorm | Euronorm Stainless Steel |
EN X6CrNiM017-13-2 |
|||||
EN X6CrNiM0Nb17-12-2 |
|||||
EN X6CrNiM0Ti17-12-2 |
|||||
EN X6CrNiNb18-10 |
|||||
EN X6CrNiTi18-10 |
|||||
EN X7CrNiTiB18-10 |
|||||
EN X8CrNiM0VNb16-13 |
|||||
EN X8CrNiNb16-13 |
|||||
EN X8NiCrAlTi32-20 |
|||||
EN X10CrNiMoMnNbVB15-10-1 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) |
---|---|---|---|---|---|---|---|
0.03 | 1.00 | 2.00 | 0.045 | 0.030 | 17.0-19.0 | 9.00-11.5 | 0.12-0.20 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
555 (≥) | 432 (≥) | 42 | 32 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
13 | - | - | 0.34 | - | |||
924 | 593 | - | 44.3 | 324 | - | ||
916 | - | 21 | 42.2 | 334 | 313 |
Heat treated : 1714°C - 1764°C
Grade | Standard | Country | Application |
---|---|---|---|
EN X2CrNiNi810KD | EN | Euronorm | Euronorm Stainless Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com