Germany DIN S18-1-2-10 High-speed tool steel and S18-1-2-10 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Tool Steel And Hard Alloy | S18-1-2-10 | DIN | Germany | High-speed tool steel |
S7-4-2-5 |
|||||
1.3246 |
|||||
S2-10-1-8 |
|||||
1.3247 |
|||||
S2-9-2-8 |
|||||
1.3249 |
|||||
S18-1-2-5 |
|||||
1.3255 |
|||||
S18-1-2-15 |
|||||
1.3257 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) | Co(%) |
---|---|---|---|---|---|---|---|---|---|
0.72-0.80 | Max 0.45 | Max 0.40 | Max 0.030 | Max 0.030 | 3.80-4.50 | 0.50-0.80 | 1.40-1.70 | 17.5-18.50 | 9.00-10.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
276 (≥) | 147 (≥) | 43 | 12 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
41 | - | - | 0.23 | - | |||
929 | 185 | - | 11.3 | 243 | - | ||
386 | - | 44 | 31.2 | 244 | 132 |
Heat treated : 1144°C - 1662°C
Grade | Standard | Country | Application |
---|---|---|---|
S18-1-2-10 | DIN | Germany | High-speed tool steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com