Germany DIN S18-1-2-15 High-speed tool steel and S18-1-2-15 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Tool Steel And Hard Alloy | S18-1-2-15 | DIN | Germany | High-speed tool steel |
| S6-5-2-5S |
|||||
| 1.3245 |
|||||
| S7-4-2-5 |
|||||
| 1.3246 |
|||||
| S2-10-1-8 |
|||||
| 1.3247 |
|||||
| S2-9-2-8 |
|||||
| 1.3249 |
|||||
| S18-1-2-5 |
|||||
| 1.3255 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | V(%) | W(%) | Co(%) |
|---|---|---|---|---|---|---|---|---|---|
| 0.60-0.70 | Max 0.45 | Max 0.40 | Max 0.030 | Max 0.030 | 3.80-4.50 | 0.50-1.00 | 14.0-17.0 | 17.50-18.50 | 15.00-16.00 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 978 (≥) | 393 (≥) | 42 | 34 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 42 | - | - | 0.11 | - | |||
| 575 | 838 | - | 23.3 | 224 | - | ||
| 818 | - | 41 | 41.2 | 112 | 213 |
Heat treated : 1719°C - 1158°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| S18-1-2-15 | DIN | Germany | High-speed tool steel |