Euronorm EN EN 25CrMoS4 Euronorm Structural steel and EN 25CrMoS4 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | EN 25CrMoS4 | EN | Euronorm | Euronorm Structural steel |
| EN C72D2 |
|||||
| EN C76D2 |
|||||
| EN C78D2 |
|||||
| EN C80D2 |
|||||
| EN C82D2 |
|||||
| EN C86D2 |
|||||
| EN C88D2 |
|||||
| EN C92D2 |
|||||
| EN C98D2 |
|||||
| EN 25CrMo4 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) |
|---|---|---|---|---|---|---|
| 0.22-0. 29 | 0.40 | 0.60-0.90 | 0.035 | 0. 020-0.04 | 00.90-1. 20 | 0.15-0. 30 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 999 (≥) | 513 (≥) | 41 | 31 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 233 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 33 | - | - | 0.12 | - | |||
| 971 | 567 | - | 22.3 | 242 | - | ||
| 128 | - | 13 | 13.2 | 424 | 233 |
Heat treated : 1341°C - 1978°C
| Grade | Standard | Country | Application |
|---|---|---|---|
| 25CrMoS4 | UNE | Spain | Spain structural alloy steel |
| EN 25CrMoS4 | EN | Euronorm | Euronorm Structural steel |