Euronorm EN EN C86D2 Euronorm Structural steel and EN C86D2 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application |
|---|---|---|---|---|---|
| Steel Grades | Structure Steel | EN C86D2 | EN | Euronorm | Euronorm Structural steel |
| EN C60D2 |
|||||
| EN C62D2 |
|||||
| EN C66D2 |
|||||
| EN C68D2 |
|||||
| EN C70D2 |
|||||
| EN C72D2 |
|||||
| EN C76D2 |
|||||
| EN C78D2 |
|||||
| EN C80D2 |
|||||
| EN C82D2 |
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
|---|---|---|---|---|---|---|---|
| 0.84-0.88 | 0.10-0.30 | 0.50-0.70 | 0.020 | 0.025 | 0.10 | 0.10 | 0.02 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
|---|---|---|---|---|---|---|
| 866 (≥) | 263 (≥) | 22 | 22 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
| Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
|---|---|---|---|---|---|---|---|
| 13 | - | - | 0.33 | - | |||
| 877 | 364 | - | 13.3 | 132 | - | ||
| 468 | - | 31 | 11.2 | 222 | 141 |
Heat treated : 1577°C - 1656°C