20MoNi35 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Cu(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|
0.27-0.23 | 0.17-0.37 | 0.40-0.80 | 0.035 | 0.020-0.040 | Max 0.30 | 3.20-3.80 | 0.20-0.30 | 0.3 | 0.02 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
811 (≥) | 187 (≥) | 21 | 22 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
21 | - | - | 0.23 | - | |||
659 | 826 | - | 33.3 | 321 | - | ||
564 | - | 33 | 34.2 | 133 | 233 |
Heat treated : 1775°C - 1351°C