Germany DIN X12CrNiSi35(36)-16 Stainless steel and X12CrNiSi35(36)-16 Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | X12CrNiSi35(36)-16 | DIN | Germany | Stainless steel |
X15CrNiSi20-12 |
|||||
1.4833 |
|||||
X12CrNi23-13/X7CrNi23-14 |
|||||
1.4841 |
|||||
X15CrNiSi25-21(20) |
|||||
1.4845 |
|||||
X8(12)CrNi25-21 |
|||||
X10CrNi32-20 |
|||||
1.4861 |
|||||
1.4864 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | N(%) |
---|---|---|---|---|---|---|---|
Max 0.15 | 1.00-2.00 | Max 2.00v | Max 0.030 | Max 0.015 | 15.0-17.0 | 33.0-37.0 | Max 0.11 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
568 (≥) | 942 (≥) | 44 | 32 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 243 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
23 | - | - | 0.32 | - | |||
164 | 286 | - | 14.3 | 244 | - | ||
449 | - | 13 | 31.2 | 342 | 331 |
Heat treated : 1612°C - 1524°C
Grade | Standard | Country | Application |
---|---|---|---|
X12CrNiSi35(36)-16 | DIN | Germany | Stainless steel |