Japan JIS SUS329J3L Austenitic-ferritic (Duplex) stainless steels and SUS329J3L Mechanical Properties, Chemical Element, Cross Reference, Datasheet.
| Category | Type | Steel Grade | Standard | Country | Application | 
|---|---|---|---|---|---|
| Steel Grades | Special Steel | SUS329J3L | JIS | Japan | Austenitic-ferritic (Duplex) stainless steels | 
| NiCr20CoMo | |||||
| NiCr18Co | |||||
| NiCr18Co | |||||
| 1.4986 | |||||
| X7(8)CrNiMoBNb16-16 | |||||
| 1.4988 | |||||
| X8CrNiMoVNb16-13 | |||||
| SUSXM7 | |||||
| SUSXM15J1 | |||||
| SUS329J1 | 
| C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | N(%) | 
|---|---|---|---|---|---|---|---|---|
| Max 0.030 | Max 1.00 | Max 2.00 | Max 0.04 | Max 0.03 | 21.0-24.0 | 4.50-6.50 | 2.50-3.50 | 0.08-0.20 | 
| Yield Rp0.2 (MPa) | Tensile Rm (MPa) | Impact KV/Ku (J) | Elongation A (%) | Reduction in cross section on fracture Z (%) | As-Heat-Treated Condition | Brinell hardness (HBW) | 
|---|---|---|---|---|---|---|
| 235 (≥) | 977 (≥) | 11 | 11 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 132 | 
| Temperature (°C) | Modulus of elasticity (GPa) | Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) | Specific thermal capacity (J/kg·°C) | Specific electrical resistivity (Ω mm²/m) | Density (kg/dm³) | Poisson’s coefficient, ν | 
|---|---|---|---|---|---|---|---|
| 14 | - | - | 0.11 | - | |||
| 663 | 134 | - | 13.3 | 324 | - | ||
| 871 | - | 43 | 21.2 | 341 | 122 | 
Heat treated : 1839°C - 1713°C
| Grade | Standard | Country | Application | 
|---|---|---|---|
| SUS329J3L | JIS | Japan | Austenitic-ferritic (Duplex) stainless steels | 