C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | Al(%) | Ti(%) | Other(%) |
---|---|---|---|---|---|---|---|---|---|---|
Max 0.10 | Max 0.50 | Max 1.00 | Max 0.03 | Max 0.015 | 20.0-23.0 | Mix 58 | 8.00-10.00 | Max 0.40 | Max 0.40 | Fe(%) Max 5.00 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
161 (≥) | 953 (≥) | 21 | 41 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
31 | - | - | 0.24 | - | |||
734 | 445 | - | 43.3 | 314 | - | ||
982 | - | 12 | 12.2 | 114 | 142 |
Heat treated : 1287°C - 1264°C