Category | Type | Steel Grade | Standard | Country | Application |
---|---|---|---|---|---|
Steel Grades | Special Steel | NCF600 | JIS | Japan | ferritic stainless steel |
NCF80A① |
|||||
NCF825 |
|||||
NCF800H |
|||||
NCF800 |
|||||
NCF751 |
|||||
NCF750 |
|||||
NCF718 |
|||||
NCF690 |
|||||
NCF625 |
|||||
NCF601 |
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Cu(%) | Other(%) |
---|---|---|---|---|---|---|---|---|
Max 0.15 | Max 0.50 | Max 1.00 | Max 0.03 | Max 0.015 | 14.00-17.0 | Mix 72.00 | Max 0.50 | Fe(%) 6.00-10.0 |
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
485 (≥) | 489 (≥) | 12 | 23 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson’s coefficient, ν |
---|---|---|---|---|---|---|---|
44 | - | - | 0.11 | - | |||
921 | 922 | - | 33.3 | 213 | - | ||
314 | - | 21 | 43.2 | 143 | 424 |
Heat treated : 1221°C - 1699°C
Grade | Standard | Country | Application |
---|---|---|---|
NCF600 | JIS | Japan | ferritic stainless steel |
NCF600TP | JIS | Japan | ferritic stainless steel |
NCF600TB | JIS | Japan | ferritic stainless steel |
CNS NCF600 | CNS | China | China Taiwan Heat-Resistant Steel |
Our main peoducts of steel are many kinds of special steel, like tool steel, mould steel, alloy steel, alloy constructural steel, heat-resistant steel, high speed tool steel,spring steel and bearing steel , stainless steel and so on, which have formed 12 series and more than 350 varieties with n...
Rfq.: sales@longhaisteel.com